Physical Properties Metric English Comments
Coating Weight >= 200 g/m²
>= 125 lb/ream
double-sided
ArcelorMittal Extragal® Z200 Double-sided pure zinc galvanized steel
Applications: Because of their high corrosion protection capacity and surface quality, Extragal® coated products are recommended for numerous automotive applications, for both visible and non-visib..
Coating Weight >= 200 g/m²
>= 125 lb/ream
double-side
ArcelorMittal ZA200 Steel coated with galfan zinc-aluminum alloy
Applications: The ductility and strong anti-corrosion properties of galfan make it a coating highly suited for deep-drawn parts and parts requiring a high level of corrosion protection. In certain ..
Coating Weight >= 200 g/m²
>= 125 lb/ream
ArcelorMittal AS200 Aluminized steel
Applications: Alusi® coating is resistant to heat, high temperature oxidation and corrosion, and offers a high level of reflectivity, making it suitable for applications in a corrosive atmosphere ..