Physical Properties Metric English Comments
Coating Weight 32.8 g/m²
20.5 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 50MO747 OPP Film
Product Description: A white opaque biaxially oriented polypropylene film, coated on one side acrylic, one side PVdC. Provides excellent performance on all packaging machines.Availability: Africa & ..