Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 20.2 g/m² | 12.6 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 33LL247 OPP Film Product Description: A super white opaque, high gloss, caviated BOPP film designed for use in reel-fed warp-around labeling applications where superior graphics are desired.Availability: Africa & Mi.. |
|||
Coating Weight | 20.2 g/m² | 12.6 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 38DL247 OPP Film Product Description: A super white opaque, high gloss, high yield and highly cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Av.. |
|||
Coating Weight | 20.2 g/m² | 12.6 lb/ream | ExxonMobil Method |
ExxonMobil Oppalyte™ 38DO447 OPP Film Product Description: A super white opaque BOPP film. The Diamex technology allows for super low density and very high yield. Diamex makes it possible to lower the density, without decreasing the mod.. |
|||
Coating Weight | 20.2 g/m² | 12.6 lb/ream | ExxonMobil Method |
ExxonMobil Oppalyte™ 33ICE OPP Film Product Description: Coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal on.. |
|||
Coating Weight | 20.2 g/m² | 12.6 lb/ream | ExxonMobil Method |
ExxonMobil Oppalyte™ 33MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |