Polymer Property : Coating Weight = 19.7 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 19.7 g/m²
12.3 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 85 AXT OPP Film
Product Description: Bicor ASB-X is a two side coated, sealable OPP film delivering an advanced level of moisture and oxygen battier protection. This film is designed for use in (unsupported and sur..