Physical Properties Metric English Comments
Coating Weight 30.7 g/m²
19.2 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 220 AB OPP Film
Product Description: Bicor AB is a two-side acrylic coated, sealable OPP film designed for general use in overwrap and horizontal packaging. It can be surface printed, reverse printed, or used unpri..