Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 30.0 - 55.0 g/m² | 18.8 - 34.4 lb/ream | |
ArcelorMittal ZF90 Galvannealed zinc-iron alloy coated steel Applications: The excellent corrosion protection and high surface quality offered by Galvannealed coatings make these products well suited for numerous automotive applications involving both visible.. |