Physical Properties Metric English Comments
Coating Weight 29.0 g/m²
18.1 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 32MB768 OPP Film
Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu..