Polymer Property : Coating Weight = 16.0 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 16.0 g/m²
10.0 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 18MM388 OPP Film
Product Description: A metallized biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance p..