Polymer Property : Coating Weight = 13.3 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 21.3 g/m²
13.3 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 30MW747 OPP Film
Product Description: White opaque biaxially oriented polypropylene film coated on one side acrylic, one side PVdC. Provides excellent performances on all packaging machines. 30MW747 is a super white..