Physical Properties Metric English Comments
Coating Weight 19.4 g/m²
12.1 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 84 AOH OPP Film
Product Description: Bicor AOH is a two-side coating OPP film designed for high oxygen barrier laminations. AOH is designed to be used as the outer web in gas-flush applications for dry products.Ava..