Physical Properties | Metric | English | Comments |
---|---|---|---|
Drawdown | 5.00 m/s @Temperature 240 °C |
984 ft/min @Temperature 464 °F |
Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escorene™ FL 00714 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00714 is an easy processable grade for extrusion coating, co-extrusion coating and cast film. This grade offers excellent heat sealing characteristics and excellent optical p.. |