Polymer Property : Drawdown = 9.10 m/s Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Drawdown >= 9.10 m/s
>= 1790 ft/min
NOVA Chemical test method
NOVA Chemicals Novapol® LC-0717-A LDPE Extrusion Resin
High speeds, Low coating weights, Excellent adhesion, Excellent drawdown, Excellent sealabilityApplications: Sugar pouch stock; Popsicle wrap, Multi-wall bags, High speed/low coating weight paper co..