Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drawdown = 6.60 m/s Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Drawdown 6.60 m/s

@Temperature 295 °C
1300 ft/min

@Temperature 563 °F
Constant output at 35 rpm; ExxonMobil Method
ExxonMobil OPTEMA™ TC 120 ExCo Ethylene Methyl Acrylate
Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer intended for extrusion coating, coextrusion coating and extrusion lamination where good interlayer adhesion between polyet..