Physical Properties | Metric | English | Comments |
---|---|---|---|
Drawdown | 2.83 m/s @Temperature 280 °C |
557 ft/min @Temperature 536 °F |
Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escor™ 5000 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5000 is primarily intended for extrusion coating, coextrusion coating, extrusion lamination. Very good adhesion to polar substrates, aluminum foil, metalized films, papers.. |
|||
Drawdown | 2.83 m/s @Temperature 280 °C |
557 ft/min @Temperature 536 °F |
Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escor™ 5020 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5020 is primarily intended for extrusion coating and coextrusion coating. Very good adhesion to polar substrates, aluminum foil, metalized films, papers, iron, steel and g.. |