Polymer Property : Neck In = 9.00 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Neck In 9.00 cm
3.54 in
Constant output 50m/min, 295°C; Internal Method
Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin
LDC801YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC801YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2..