Polymer Property : Neck In = 5.50 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Neck In 5.50 cm
2.17 in
at 1000 ft/min; Neck-in reported is the total of both sides; NOVA Chemicals test method
NOVA Chemicals Novapol® LC-0717-A LDPE Extrusion Resin
High speeds, Low coating weights, Excellent adhesion, Excellent drawdown, Excellent sealabilityApplications: Sugar pouch stock; Popsicle wrap, Multi-wall bags, High speed/low coating weight paper co..