Polymer Property : Kinematic Viscosity = 80 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity 80 cSt

@Temperature 20.0 °C
80 cSt

@Temperature 68.0 °F
ASTM D445
Solvay Specialty Polymers FOMBLIN® LC80 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..