Polymer Property : Kinematic Viscosity = 64 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity 64 cSt

@Temperature 20.0 °C
64 cSt

@Temperature 68.0 °F
ASTM D445
Solvay Specialty Polymers FOMBLIN® Y L-VAC 06/6 PFPE Pump Oil
FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and..