Polymer Property : Kinematic Viscosity = 6.14 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity 6.14 cSt
6.14 cSt
ASTM D445
ExxonMobil Exxsol™ D140 Dearomatized Fluid
Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil