Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 562 cSt | 562 cSt | |
Dow Corning FZ-7604 Dow Corning® FZ-7604 is a 100% solids silicone polyether that shows good compatibility with water-based formulations. It provides effective slip and mar resistance enhancement performance and broad.. |