Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 340 cSt @Temperature 25.0 °C |
340 cSt @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 7044 COATING Syl-Off® 7044 Coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity vinyl endblocked and pendant functional silicone polymer. Pre-catalysed with Rhodium catalyst. Re.. |