Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 3000 cSt @Temperature 25.0 °C |
3000 cSt @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 7012 RELEASE MODIFIER Syl-off® 7012 Release Modifier is a 100% active solids, pre-catalysed, release modifier. Offers particularly smooth release modification.Information provided by Dow Corning |