Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 3.8 cSt @Temperature 25.0 °C |
3.8 cSt @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® LLS215 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |