Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 22.1 cSt | 22.1 cSt | |
Dow Corning FZ-77 Dow Corning® FZ-77 is a 100% solids silicone polyether that shows good compatibility with water-based formulations. It provides leveling and wetting performance, enhances gloss, and improves mar re.. |