Polymer Property : Kinematic Viscosity = 20.1 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity 20.1 cSt

@Temperature 21.0 °C
20.1 cSt

@Temperature 69.8 °F
ASTM D 445
ConocoPhillips Hydroclear® 10 Ultra-Clean Spindle Oil
Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties o..