Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 2.02 cSt | 2.02 cSt | ASTM D445 |
ExxonMobil Isoparâ„¢ L (AM) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Central America, South Amer.. |