Polymer Property : Kinematic Viscosity = 1970 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity 1970 cSt

@Temperature -40.0 °C
1970 cSt

@Temperature -40.0 °F
ASTM D445
ExxonMobil Exterex™ A34 Synthetic Fluid
Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol..