Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 18.9 cSt @Temperature 25.0 °C |
18.9 cSt @Temperature 77.0 °F |
ASTM D445 |
PolyOne Synplast™ DOS-N Di (2-ethylhexyl) Sebacate Branched C8 sebacate esterInformation provided by PolyOne |