Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 17.3 cSt @Temperature 25.0 °C |
17.3 cSt @Temperature 77.0 °F |
ASTM D445 |
PolyOne Synplast™ DINA-N Di Isononyl Adipate Branched C9 adipate esterInformation provided by PolyOne |