Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 160 cSt @Temperature 20.0 °C |
160 cSt @Temperature 68.0 °F |
ASTM D445 |
Solvay Specialty Polymers FOMBLIN® Z15 PFPE Lubricant FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc... |