Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 135 cSt | 135 cSt | |
Dow Corning SYL-OFF® SL 9110 COATING Syl-Off® SL 9110 Coating is a solvent-free release coating for filmic pressure sensitive laminate/labelstock, exceptionally low temperature cure.Information provided by Dow Corning |