Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | >= 110 cSt | >= 110 cSt | |
Kazanorgsintez Dust Suppressor "M", Modified Polyethyleneglycolether Mixture Production Method: Mixture of polyethylene glycol ethers. Application: Intended for use as a reactant in the production of potassic fertilizers to decrease dust formation in ore mining plants and to.. |