Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 1.61 cSt | 1.61 cSt | ASTM D445 |
ExxonMobil Isopar™ L (AP) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Asia PacificInformation pro.. |
|||
Kinematic Viscosity | 1.61 cSt | 1.61 cSt | ASTM D445 |
ExxonMobil Varsol™ 140 Naphtha Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |