Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 0.93 cSt | 0.93 cSt | ASTM D445 |
ExxonMobil Varsolâ„¢ 30 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil |