Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 0.75 cSt @Temperature 25.0 °C |
0.75 cSt @Temperature 77.0 °F |
NULL |
Solvay Specialty Polymers PERFLUOROSOLVâ„¢ PFS1 Perfluorinated Cleaning Solvent PERFLUOROSOLV PFS-1 is a low molecular weight perfluoropolyether solvent and diluent that perfroms well in many electronic and semiconductor cleaning functions, such as: pump cleaning, degreasing, d.. |
|||
Kinematic Viscosity | 0.75 cSt | 0.75 cSt | |
3M Fluorinert™ FC-3283 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3283 is a non-conductive, thermally and chemically stable liquid ideal for use in single phase heat transfer applications, especially in the electronics and semiconductor.. |