Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 0.70 cSt | 0.70 cSt | |
Dow Corning Z-1213 N-PROPYLTRICHLOROSILANE n-propyltrichlorosilane fluidInformation provided by Dow Corning |
|||
Kinematic Viscosity | 0.70 cSt | 0.70 cSt | |
Dow Corning Z-6264 SILANE Dow Corning® Z-6264 Silane is an alkylalkoxysilane. It has an n-propyl organic group and a trimethoxysilyl inorganic group.Information provided by Dow Corning |
|||
Kinematic Viscosity | 0.70 cSt | 0.70 cSt | |
Dow Corning Z-6518 SILANE Dow Corning® Z-6518 Silane is an organofunctional reactive silane. The product have a vinyl reactive organic group and a trimethoxysilyl or triethoxysilyl reactive inorganic group. Dow Corning® Z-.. |