Physical Properties Metric English Comments
Kinematic Viscosity 0.57 cSt

@Temperature 25.0 °C
0.57 cSt

@Temperature 77.0 °F
Solvay Specialty Polymers Galden® SV80 PFPE Solvent
Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature..