Density 9.78 - 9.98 g/cc
0.353 - 0.361 lb/in³
MarkeTech Cu/Mo/Cu 13:74:13 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..