Polymer Property : Density = 9.81 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 9.81 g/cc
0.354 lb/in³
Indium Corp. Indalloy 160-190 Fusible Bismuth Alloy
Information Provided by Indium Corporation