Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.52 - 10.13 g/cc | 0.344 - 0.3660 lb/in³ | as sintered |
H.C. Starck Molybdenum Alloy PSBT P/M TZM Powder Metallurgy Billet Description of Product: This specification covers molybdenum alloy (molybdenum + 0.5% titanium + 0.1% zirconium) pressed and sintered billet.Physical Properties: Density: The as-sintered density w.. |
|||
Density | 9.52 g/cc | 0.344 lb/in³ | |
Lucas-Milhaupt EASY FLO 3 Carbide Brazing Alloy Easy-Flo 3 is recommended for use on stainless steels subject to chloride corrosion, such as marine hardware, fishing tackle, and some dairy equipment cleaned with bleaching solutions and other equi.. |