Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.30 - 9.50 g/cc | 0.336 - 0.343 lb/in³ | |
MarkeTech Mo50Cu Moly/Copper Heat Sink Material MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivit.. |
|||
Density | 9.30 g/cc | 0.336 lb/in³ | |
Indium Corp. Indalloy 217-440 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.30 g/cc | 0.336 lb/in³ | |
Indium Corp. Indalloy 83 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.30 g/cc | 0.336 lb/in³ | |
Lucas-Milhaupt Silvaloy® 35 Brazing Alloy Silvaloy 35 is an alloy with a melting range suitable for brazing steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It is free-flowing and suited .. |
|||
Density | 9.30 g/cc | 0.336 lb/in³ | |
Indium Corp. Indalloy® 206 Pb-In Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Density | 9.30 g/cc | 0.336 lb/in³ | |
Williams Advanced Alloys WS225 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |