Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.20 g/cc | 0.332 lb/in³ | |
Indium Corp. Indalloy 78 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.20 g/cc | 0.332 lb/in³ | |
Lucas-Milhaupt BRAZE 452 Characteristics:Braze 452 is a free-flowing, low temperature filler metal commonly used to replace cadmium-bearing filler metals of similar silver content. This alloy is best suited for narrow gap .. |