Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.17 g/cc | 0.331 lb/in³ | |
Indium Corp. Indalloy 126 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.17 g/cc | 0.331 lb/in³ | |
Lucas-Milhaupt BRAZE 505 Carbide Brazing Alloy Applications: Braze 505 readily wets nickel and iron base alloys. It is recommended for joining 300 Series stainless steel and will retard interface corrosion in most exposures for which the base m.. |