Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.10 g/cc | 0.329 lb/in³ | |
Wall Colmonoy WALLEX 50 - Cobalt-Nickel Alloy Description: Good corrosion resistance and low coefficient-of-friction provides good metal-to-metal wear protection (not involving much impact). For bushings, knives and cams. Finished by grinding.. |