Physical Properties Metric English Comments
Density 8.96 g/cc
0.324 lb/in³
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy
Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu..
Density 8.96 g/cc
0.324 lb/in³
Goodfellow Magnetic Copper Alloy
Information provided by Goodfellow.