Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.62 g/cc | 0.311 lb/in³ | |
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022 AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provide.. |