Polymer Property : Density = 8.24 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 8.24 g/cc
0.298 lb/in³
Wall Colmonoy COLMONOY® 52 SA - Hard Nickel-Chromium-Boron Alloy Containing Chromium Carbides
Description and Application: Similar to Colmonoy No. 62 SA, but has increased ductility with almost the same abrasion and corrosion resistance. Finished by grinding.Method of Application: Sprayweld..
Density 8.24 g/cc
0.298 lb/in³
ATI Allvac® M-252 Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal
Applications: Turbine blades, fasteners, and high temperature bolting.Data provided by Allvac.
Density 8.24 g/cc
0.298 lb/in³
ATI Allvac® Nickelvac® W-722 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age
Data provided by Allvac.Applications: Ring components in jet engines.
Density 8.24 g/cc
0.298 lb/in³
ATI Allvac® Nickelvac® X- 751 UNS N07751 Nickel Superalloy
Uses: Components for gas turbine engines, exhaust valve stock for internal combustion engines.Property values are for samples in the metallurgical condition: 1800°F age.Information provided by Allv..
Density 8.24 g/cc
0.298 lb/in³
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age
Data provided by Allvac.Applications: Jet and rocket engines, torque rings, afterburners, and hardware; space shuttle turbo pumps seals.
Density 8.24 g/cc
0.298 lb/in³
Wall Colmonoy COLMONOY® 5 - Hard-Surfacing Alloy Containing Wear-Resistant Chromium Borides and Carbides
Description: Contains wear-resistant chromium borides and carbides. Has greater ductility, better impact resistance and workability than Colmonoy No. 6 Finished with carbide tools and grinding.App..