Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.21 g/cc | 0.297 lb/in³ | |
Special Metals NIMONIC® Alloy PK33 A nickel-chromium-cobalt alloy that is precipitation hardenable and also contains a relatively high (7%) level of molybdenum for solid-solution strengthening. It has an exceptional combination of h.. |
|||
Density | 8.21 g/cc | 0.297 lb/in³ | |
Special Metals UDIMET® alloy 520 Superalloy UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris.. |