Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.06 g/cc | 0.291 lb/in³ | |
Indium Corp. Indalloy 230 Indium-Tin-Lead Solder Alloy Also known as 532Information Provided by Indium Corporation |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
Indium Corp. Indalloy 532 Tin Solder Alloy Also known as 230Information Provided by Indium Corporation |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
Special Metals NIMONIC® Alloy 81 A precipitation-hardenable nickel-chromium alloy with enhanced resistance to high-temperature corrosion. The excellent hot-corrosion resistance of the alloy results from its high chromium content o.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
Wall Colmonoy COLMONOY® 69 SC - Alloy With Chromium Carbide Description and Application: Enhanced Colmonoy 69, with more chromium and molybdenum for better corrosion resistance. Improved plastic range makes overlays easier to fuse without sagging. For mari.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
Carlson 20 Plus Alloy Carlson C20 Plus is a super-austenitic alloy, developed to provide maximum resistance to corrosion by sulfuric acid. Nickel chromium, molybdenum and copper contribute to the excellent overall resist.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367) The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
ATI Allvac® AL 6XN® UNS N08367 Specialty Steel Uses: Process equipment, flue-gas scrubber systems, multi-effect evaporators for brines, seawater, pulp & paper liquors.Property values are for samples in the metallurgical condition: 2050°F anneal.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 10% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 20% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 30% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 40% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 50% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 60% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Density | 8.06 g/cc | 0.291 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 75% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |