Physical Properties Metric English Comments
Density 8.0 - 8.1 g/cc
0.29 - 0.29 lb/in³
EOS MS1 Maraging Steel for DMLS 3D Printing
EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us..